Key takeaways
- Hydrostatic pressure and impact penetration tests measure resistance to water; wet and dry microbial penetration tests measure resistance to micro-organisms.
- Each test simulates a different mechanism of strike-through, so a strong result in one does not guarantee a strong result in another.
- For some tests a higher number is better and for others a lower number is better, which makes the unit and direction essential when reading a report.
- Results apply to the specimens tested, so check that the report describes the finished, sterilised product you intend to buy.
A specification for a surgical gown or drape often comes down to a handful of test results. The names are technical and the units are unfamiliar, yet these results are what a performance class or barrier level actually rests on. This article describes four of the most commonly cited barrier tests in plain terms: what the laboratory does, what the number means, and what the test cannot tell you. Pass limits vary by standard and by product area and are not quoted here; they should be taken from the current edition of the standard named in your specification.
Why more than one test is needed
Liquid and micro-organisms can cross a fabric by different routes. A splash strikes the surface briefly. A pool of irrigation fluid sits on a drape and is pressed into it by a forearm. Dry skin scales and dust settle and are shaken through open pores. Bacteria on a wet surface are driven through by rubbing. No single test reproduces all of these, so standards combine several.
They also divide by framework. European and Indian practice draws on ISO test methods, while the American classification uses AATCC and ASTM methods. The principles overlap, but results from one method cannot be read across to another.
Hydrostatic pressure: resistance to sustained liquid
In the hydrostatic pressure test, often called the hydrostatic head test, a specimen is clamped over a reservoir so that one face is in contact with water. The pressure of the water is increased at a steady rate while the technician watches the other face. The pressure at which water breaks through is recorded.
The result is expressed as the height of a column of water, usually in centimetres. A higher figure means greater resistance. This test represents situations in which liquid is held against the material under pressure, such as leaning on a wet drape or resting an arm in pooled fluid. It is carried out according to methods such as ISO 811 or AATCC 127, depending on the framework.
It is a test of the material in a small flat area. Seams, sleeve joints and the edges of reinforcements behave differently and need to be considered separately.
Impact penetration: resistance to spray and splash
The impact penetration test, AATCC 42, belongs to the American framework. A specimen is mounted on an inclined surface with a pre-weighed sheet of blotting paper behind it. A measured volume of water is sprayed onto the specimen from a set height. The blotter is then weighed again, and the increase in weight shows how much water passed through.
The result is a weight in grams, and here a lower figure is better. The test models a brief splash or spray without sustained pressure. It is the basis of the lower levels of the AAMI classification, with the hydrostatic pressure test added as the levels rise. A fabric can perform well against spray and still give way under sustained pressure, which is why the two are used together.
Microbial penetration: wet and dry
Wet: bacteria carried through by liquid and friction
Water resistance is an indirect measure. The wet microbial penetration test, ISO 22610, looks directly at bacteria. The test material is placed on an agar plate. A carrier material contaminated with a known bacterial suspension is laid on top, and a weighted finger rubs across the assembly for a set time, combining moisture, pressure and friction. The procedure is repeated on a series of fresh plates, and after incubation the bacterial colonies that have come through are counted.
From these counts a barrier index is calculated. A higher index indicates a better barrier, and the maximum value indicates that no penetration was detected. This test is applied to the critical areas of a product, the parts expected to become wet and to be handled, and it is one of the main points on which the European high performance class differs from standard performance.
Dry: particles through a dry fabric
The dry microbial penetration test, ISO 22612, addresses the opposite condition. Talc powder carrying bacterial spores is placed on the specimen, which is mounted over an agar plate. The apparatus is vibrated so that the powder is shaken against the fabric, and any spores that pass through fall onto the plate. After incubation the colonies are counted.
The result is a count of colony forming units, and a lower count is better. This test is applied to less critical areas, which are expected to remain dry. It reflects the fact that an open, breathable fabric may resist liquid moderately well yet still allow fine dry particles to pass.
The four tests side by side
| Test | Typical method | Challenge | Result expressed as | Better result |
|---|---|---|---|---|
| Hydrostatic pressure | ISO 811; AATCC 127 | Water under rising pressure | Height of water column | Higher |
| Impact penetration | AATCC 42 | Water sprayed onto the surface | Weight of water passing through | Lower |
| Wet microbial penetration | ISO 22610 | Bacteria in liquid, with rubbing | Barrier index | Higher |
| Dry microbial penetration | ISO 22612 | Spores on dry powder, with vibration | Colony count | Lower |
For the highest American level, further tests apply: resistance to synthetic blood and to penetration by a virus surrogate under ASTM methods. These are pass or fail tests and are the reason that level is treated as a distinct step, not simply a higher number on the same scale.
Reading a test report, and what to ask your supplier
When a report arrives, check the following before looking at the numbers:
- The test method and its edition, and whether the laboratory is accredited for that method.
- The description of the sample: product code, fabric construction, weight, and whether it was tested after sterilisation.
- Which area of the product the specimens were cut from, and whether seams were included.
- The number of specimens and whether individual values or only an average is shown.
- The date of the report and whether the material or supplier has changed since.
Then ask the supplier how often testing is repeated and how incoming fabric is checked between full tests. Shrisay Medical manufactures surgical gowns and surgical drapes to customer requirement; if you need test evidence for a particular configuration, raise it at the enquiry stage through our contact page so that the requirement is clear before a sample is made.
Frequently asked questions
What does a hydrostatic head figure mean?
It is the height of a water column the material resisted before water penetrated, usually given in centimetres. A higher figure indicates greater resistance to liquid under sustained pressure.
Why are wet and dry microbial penetration tested on different parts of a product?
Critical areas are expected to become wet and to be rubbed, so wet penetration is the relevant risk. Less critical areas are expected to stay dry, so penetration by dry particles is tested there.
Can I compare an ISO 811 result with an AATCC 127 result?
Both measure resistance to hydrostatic pressure, but the methods and conditions are not identical. Compare results obtained by the same method, and use the method named in the standard you are specifying.